search  current discussion  categories  kilns & firing - wood 

wood on gas kiln

updated sat 10 aug 02

 

Jorge Nabel on fri 9 aug 02


Mel wrote
""i love wood. i stuff small pieces of wood into my kiln when it is
finished firing. close it all down, and insert the wood in the burner
ports. i can pull back my burners, so it is easy. then close up the kiln
and let it smoke. ""

Major, I put a garlic in my first gas firing(kind of superstition)and when I
opened the kiln I found some kind of ash glaze on the shelf.So, dont you
have same problem with the wood???How do you preserve the shelves??

Jorge en Buenos Aires