search  current discussion  categories  kilns & firing - misc 

new kiln working?

updated thu 8 aug 02

 

kymudworks on wed 7 aug 02


check to see if the plug you are using is powered by a big enough =
breaker for the kiln. electricians have told me to always use a breaker =
that is 15 amps or so larger than what the manual says the kiln will =
draw. i agree about getting a wiring schematic. i bought a new kiln and =
it never fired right till i discovered (long process) that it came from =
the manufacturer incorrectly wired. it happens.....