Standard Ceramics has crystals to add to low fire glazes. I've used the green
and blue and they have worked fairly well.

Another thought would be to try using glass frit from Bullseye Glass or from
Hudson Glass companies. The coeffient of expansion may be a problem between
the frit and glaze but on non-functional pieces it may be okay. Experiment to
see.