search  current discussion  categories  glazes - misc 

recipe for extrudable kiln post clay

updated fri 12 jul 02

 

Lindemann on thu 11 jul 02


CLAYART Digest - 9 Jul 2002 to 10 Jul 2002 (#2002-189)I have this recipe =
from an OLD CM for extrudable kiln post clay.

XX Saggar Clay- 25%
Kaolin---------------25%
Stoneware Grog 50%

Extrude into tubes for kiln posts.

I haven't personally tried it, but jotted it in my sketchbook for future =
reference long ago.

take care!
Pat Lindemann
Custer, SD