giffin grip not working. need some help!

updated sat 29 jun 02

 

Katheleen Nez on fri 28 jun 02


Dear June: The "o-ring" is semi-important becuz my
Giffin woudnt work when my o-ring cracked and then
broke. They will send you one for free. Also, take yer
Grip apart periodically and make sure it's clean
(remove all trimmings, caked clay from grooves). This
always seems to help.
Rock On, nezbah
note: The "slidey" feet need to be clean, too