Pancioli on mon 10 jun 02

Hi Lori:

I am working on Cone 6 reduction glazes and bodies this summer (among
other things). I should have something good to report by September. We
already have a good cone 6 body, just not the color I want. I make it
from scratch. Are you looking for a formula?

We have been working at Cone 6 reduction here at the EMU studio for a
year and have tested many glazes. I am in the process of narrowing them
down and finding the best, tweaking the formulae, etc. Takes time.