Here's the glaze, straight from James Watkins.

Hi, Dannon.
>I don't remember where the Yellow Maybe comes from. Here is the glaze. It
is
>a come 10 reduction glaze.

>Yellow Maybe
>Neph. Sye. 1908
>Dolomite 633
>Ball Clay 129
>Bentonite 240
>Zircopax 375
>Tin Ox. 70
>Red Iron Ox. 15
>
>You can get a creamy white yellow if you only add 7.5 of Red Iron.