currie method, oil spot, cobalt greens and workgroups

updated sat 1 jun 02

 

Valerie Hawkins on thu 30 may 02


Ok, Ok, I'm convinced. I'm going to place an order for Ian's book as soon
as I send this letter. I have to admit that I find the prospect of using
the 'Currie' method a bit daunting, so, I'd be interested in an workgroup if
someone else is.

Thanks to all on the oil spot, cobalt green advice and recipes!

Valerie
Charlotte

Ian Currie on fri 31 may 02


> Ok, Ok, I'm convinced. I'm going to place an order for Ian's book as soon
> as I send this letter.

One book speeding your way as I type this. Thanks for the order!

> I have to admit that I find the prospect of using
> the 'Currie' method a bit daunting, so, I'd be interested in an workgroup
if
> someone else is.

I will be posting a copy of my schedule for the Fall workshop tour soon.
Also there was a post yesterday from someone wanting to start up something
on-line again like the one Ruth Ballou organized several years ago. I will
follow that up as I read through my mail.

> Thanks to all on the oil spot, cobalt green advice and recipes!

Think twice before you post a query to Clayart. Behind the door there are
all these eager people waiting to burst into your life! :)

Regards

Ian
http://ian.currie.to/

John Weber on fri 31 may 02


Ian Currie wrote:
>I will be posting a copy of my schedule for the Fall workshop tour
soon.
Also there was a post yesterday from someone wanting to start up something
on-line again like the one Ruth Ballou organized several years ago. I will
follow that up as I read through my mail.<
I am in the process of learning and testing glazes with the grid method and
would welcome the opportunity to be involved in a group testing and sharing
results. My tests would mostly be to Cone 10 in reduction.