travis kilgore on wed 8 may 02


Ron what i am really looking for is about a cone 9-10 body i have several
cone 6 bodys that i found in the cushing handbook i would really like
something inbetween a porcelain and a white stoneware with low shrinkage
highly plastic and smooth in texture. production cost i guess might also be
a factor
thanks barbara kilgore
tkilgore@farmerstel.com
Pisgah, AL USA
----- Original Message -----
From: Ron Roy
To:
Sent: Monday, May 06, 2002 9:25 PM
Subject: Re: white stone wear formulas


> Again - it is impossible to formulate a clay that will be servicable at
> both these temperatures.
>
> RR
>
>
> >I am looking for cone 6-10 white stonewear formulas to test if anyone has
> >any good ones send them my way'
>
>
> Ron Roy
> RR #4
> 15084 Little Lake Road
> Brighton
> Ontario
> Canada - K0K 1H0
> Phone: 613-475-9544
> Fax: 613-475-3513
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>