updated sun 28 apr 02

 

Tommy Humphries on fri 26 apr 02


I have never fired the shelves by themselves with just kilnwash...just ma=
ke
sure that you take the first firing fairly slow, so that the shelves dry =
out
completely before goosing the gas...you don't want to blow up a shelf...

Tommy


----- Original Message -----
From: "Martin Rice"

Hi,

Just put kilnwash on my shelves for the first time. The simple question f=
or
today is do I have to fire the shelves by themselves before I do a glaze
firing?

Thanks so much.
Martin
Lagunas de Bar=FA, Costa Rica
www.rice-family.org
Revised and updated 4/1/02

Martin Rice on fri 26 apr 02


Hi,

Just put kilnwash on my shelves for the first time. The simple question =
for today is do I have to fire the shelves by themselves before I do a =
glaze firing?

Thanks so much.
Martin
Lagunas de Bar=FA, Costa Rica
www.rice-family.org
Revised and updated 4/1/02