Craig -

You're forgiven!!! It's a lesson I learned the hard
way and yes, it's great to be rid of the micro bubbles
that can occur without blunging (preferrable in HOT
water) the night before. Actually it was macaloid
which I put in my porcelain clay body which was
originated by Jean Otis and modified by Val Cushing.

I've only gotten one commercial clay supplier (Frank
Tucker) to even consider doing this in a custom mix
order. Everyone else thinks I'm crazy. Or it doesn't
"fit the operation." Thank you for your feedback and
support.


=====
Karen Gringhuis
KG Pottery
Box 607 Alfred NY 14802