search  current discussion  categories  glazes - misc 

vince pitelka's terrasig recipe

updated fri 15 feb 02

 

Lynne Hancox on thu 14 feb 02


Hello
Could I get some information on vince pitelka's terrasig recipe? I have
read that this is the best to use. Also, any other recipes that would give
a good "shine" to smoked pots.

Thank you in advance. This is my first time for this, so I hope I did it
right!!

Lynne

vince pitelka on thu 14 feb 02


> Could I get some information on vince pitelka's terrasig recipe? I have
> read that this is the best to use. Also, any other recipes that would
give
> a good "shine" to smoked pots.

Lynne -
My article on terra sig is on Tony Hansen's Digitalfire website at
www.digitalfire.com/education/glaze/terasig.htm
Best wishes -
- Vince

Vince Pitelka
Appalachian Center for Crafts
Tennessee Technological University
1560 Craft Center Drive, Smithville TN 37166
Home - vpitelka@dtccom.net
615/597-5376
Work - wpitelka@tntech.edu
615/597-6801 ext. 111, fax 615/597-6803
http://www.craftcenter.tntech.edu/