itc on kiln lid

updated sat 2 feb 02

 

Joseph Dallas on fri 1 feb 02


Hey Mel or other ITC users,
I just got ITC to spray my old Paragon A99 electric. I
understand your instructions and ITC's for cleaning and
spraying the kiln. My question is do you spay the lid
and the top of the walls where they touch the lid?

Snail Scott on fri 1 feb 02


At 08:56 AM 2/1/02 -0500, you wrote:
>...My question is do you spay the lid...

If you didn't, would it make lots of little lids?
(Help control the lid population!)