search  current discussion  categories  materials - misc 

apologies snail . re: gold (ot:ceramic glaze ingredients...)

updated sun 13 jan 02

 

Khaimraj Seepersad on fri 11 jan 02


Good Day to All ,

Snail ,

please accept my apologies for a non reply , my
behaviour was inexcusable .

This is exactly what I needed to hear. I had actually
theorised that Titanium would harden Gold and give
it much greater durability [ scratch resistance ].

Wow , as little as 0.5 % , to get 18 k in gold hardness.
Here I was about to cook in around 20 to 50 % Titanium.
Well time to get down and actually do the deed.
Thanks a million .
Khaimraj



-----Original Message-----
From: Snail Scott
To: CLAYART@LSV.CERAMICS.ORG
Date: 19 December 2001 14:02
Subject: Re: gold (OT:Ceramic Glaze Ingredients...)


>At 11:55 AM 12/17/01 -0800, Khaimraj wrote:
>>Can I alloy Tin and Titanium , or Gold and Titanium or
>>Silver and Titanium ?
>
>My wedding ring (made by a friend) is made of a gold/
>titanuim alloy. It is a proprietary technique, but it
>involves alloying pure gold with .5% of titanium, so
>it still assays as 24 karat gold, with the true color
>of 24 karat, but with the hardness of a standard 18
>karat alloy, which makes it more suitable for the rough
>use that hand jewelry tends to get.
>
> -Snail
>