search  current discussion  categories  glazes - crazing & crackle 

: re: help urgently needed for crazed saltglazed tiles

updated sun 30 dec 01

 

iandol on fri 28 dec 01


Dear Michael Banks <>

In response to Vivek you say <fault. But (presuming that your glaze recipe hasn't changed), >>

What glaze recipe are you talking about? This Vivek Patel said he was =
were salt glazing so it is the reaction of the sodium chloride with the =
clay which makes the glaze. Nothing is put on the clay. There is no =
glaze recipe to change!

As You may know, Glazes produced by "Vapor Glazing" with Salt always =
tend to craze. Any that do not are unusual.

Best regards,

Ivor.