marcia's redux. glazes in ox.

updated sun 9 dec 01

 

Alisa og Claus Clausen on sat 8 dec 01


All the the recipes Marcia posted some time ago showed good results in
oxidation.
The only two that were brown were the Ohata red and Sexy black. Thanks for
those recipes, Marcia,
esp. the Turquoise. I use that one a lot for vases. All recipes, both the
original posting from
Marcia and the tests I did in ox. , are the archives.

It is very busy here now, but the good news is I have been stocking up ware
since July.
So, now I have a lot of stress/guilt free time having fun in the store. My
store is as proportionately
small as my studio. Cozy as they say here. Better to have a lot of energy
and ideas and little space than a lot of space and no energy, if one must
choose. Of course I would like the ideal...a big farm and big energy.

Have a good day Clayart, I am feeling happy in cold, cold, frosty Denmark.
Alisa