Hi all, I bought some XX saggar clay, Fire clay and Grollegg, because
I wanted to make some saggars. I thought those were the ingredients in
a saggar recipe that I saw on clayart. However, now I can't find the
recipe. Unfortunately, searching the list by using groups.yahoo.com
doesn't always return what I know is there. Is there a better way to
search?

If anyone has a good saggar recipe for earthenware-midfire temps,
would you send it along? I know that at low temps a stoneware clay
would probably do, you don't have to tell me that. I want to use a
saggar clay so that I can make them once and use them until I'm 50.

Thanks, -J

"There are no pots, there is only clay." -me

chris clarke on mon 19 nov 01


Hey Jonathan,

Go to google.com and type in what you want then clayart. It will turn up
all the threads. Don't forget clayart, it's at the bottom of every post so
it cuts it down just us.

chris


temecula, california
chris@ccpots.com
www.ccpots.com




----- Original Message -----
From: Jonathan Pennington
To:
Sent: Monday, November 19, 2001 11:45 AM
Subject: Saggar clay recipe?


> Hi all, I bought some XX saggar clay, Fire clay and Grollegg, because
> I wanted to make some saggars. I thought those were the ingredients in
> a saggar recipe that I saw on clayart. However, now I can't find the
> recipe. Unfortunately, searching the list by using groups.yahoo.com
> doesn't always return what I know is there. Is there a better way to
> search?
>
> If anyone has a good saggar recipe for earthenware-midfire temps,
> would you send it along? I know that at low temps a stoneware clay
> would probably do, you don't have to tell me that. I want to use a
> saggar clay so that I can make them once and use them until I'm 50.
>
> Thanks, -J
>
> "There are no pots, there is only clay." -me
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>

Marta M. Gloviczki on mon 19 nov 01


Jonathan Pennington wrote:

>I want to use a
>saggar clay so that I can make them once and use them until I'm 50.
>

jonathan,
it all depends... how old are you?... and how many times are you
planning to fire in those saggars? :-))