purple glaze tested

updated fri 9 nov 01

 

Lesley Alexander on wed 7 nov 01


Emily's Purple tested for a release of cobalt at .03 mg/L in a batch
I sent to Alfred's. Apparently there is no standard for cobalt in
drinking water, but personally I wouldn't use it for food.
I have a number of other glazes that were sent back there in June,
and when I get the results for all of them I'll post them. Hopefully by
2002! Lesley