search  current discussion  categories  techniques - throwing 

sv: re: veg oil in water, was throw it dry

updated mon 22 oct 01

 

Isak Isaksson on sun 21 oct 01


Hi,
The best way to throw "almoust dry" is to add one spoon of
washing-up liquid, like Yes, in the water, great and keep you fingers =
clean.
(For Haloween, take 3 spoons and add some red candy-colour..)
All the best

Isak Isaksson
Velamsund
SE-132 36 S-Boo
Sweden
+46 8 747 97 21
www.swedcrafts.nu


----- Original Message -----=20
From: Lee Love
To:
Sent: Sunday, October 21, 2001 6:04 AM
Subject: Re: Veg oil in water, was Throw it dry


> ----- Original Message -----
> From: "Dannon Rhudy"
>=20
> > .....>Anyone have any thoughts about this oil in the throwing water? =
I am
> > very
> > >curious about this.......
> >
> > It can't be much trouble to try it - let us know what you think,
> > and whether the experience was positive or not.
>=20
> Wouldn't be a good idea if you want to add slips before firing.
>=20
> --
>=20
> Lee Love
> Mashiko JAPAN Ikiru@kami.com
> Interested in Folkcraft? Signup:
> Subscribe: mingei-subscribe@egroups.com
> Or: http://www.egroups.com/group/mingei
> Help ET phone Earth: http://setiathome.ssl.berkeley.edu/
>=20
> =
_________________________________________________________________________=
_____
> Send postings to clayart@lsv.ceramics.org
>=20
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>=20
> Moderator of the list is Mel Jacobson who may be reached at =
melpots@pclink.com.
>=20