Mark Lendsey on tue 16 oct 01


what is the best combination 04 body/06 clear glaze for white functional
wheel thrown ware?
i have been using lead free commercial bodies and glaze
i have glaze fired 06 glaze to 04 and got bubbles and craters
it works better to fire 06 glaze to 06
ive tried the 60/40 frit/ball clay glaze too tan and some bubbling
studio too small to mix clays and glazes at this time
i use underglazes and slips w/clear over
starting out small here at the edge of the earth florida