search  current discussion  categories  glazes - cone 4-7 

in my site in: glaze test (^6 ox.) page 2

updated sat 13 oct 01


Ababi on sat 13 oct 01

In my site in: GLAZE TEST (^6 ox.) page 2 I added pictures. The last 8
slides are about the tests I grabbed today, in my time, yesterday, from
the kiln. with explanation includes very low cost glazes- experimentally
I will answer to questions( if you will ask )
Ababi Sharon
Kibbutz Shoval- Israel
officially Glaze addict