Ron & Nancy on tue 18 sep 01

Just a note of use my first set of bowls, I made were low fire
glazes, low fire bisque. I used them for 8 years then pass them on to my
sister-in-law. She is still using them. And while they were in my house
hold they were used in the micro-wave and dish washer. While I don't
sell functional low fire, I am not sure any potter could assure a buyer
of longer use.
Respectfully, Nancy