I took a plastic light switch plate and scanned it in my scanner. Then I
used the scanner software to increase the size of the image as much as the
percentage of clay shrinkage, having previously tested my clay shrinkage.
Then I used the resultant image as a pattern to cut the holes. Everything
lined up perfectly.

Denver, NY