Lyn Peelle on sun 29 jul 01


I've just tested Andie's Handful of Earth Glaze. I htought it was a cone 6
glaze. My kiln (which is quite old ) misfired and only reaced about 1800 F
with is around cone 05-the glaze looks mature at that temp. HERE's my
problem---I can't remember where I got this glaze recipe -- I must have had
a brain cramp and didn't write the source down. Does anyone out there know
of this glaze? What cone is it good too? TIA for anyone's h