In my Quest for simple glazes i use ash a lot. mostly 50% ash 50% red clay.
Some i use red art some i use cave clay.

I just did another test using 100 grms Plastic Vitrox and 100 Grms Ash. I
added 3 grms of Cobalt Carb at cone 10 Reduction and wow is it a yummy blue.
I am using Highwaters Wonder White.

If any body tries it let me know. I love blue

Capt Mark

Edouard Bastarache on thu 19 jul 01


Hello Capt Mark,

is your ash washed? If so, how many times?

Later,


Edouard Bastarache
Irreductible Quebecois
Sorel-Tracy
Quebec
edouardb@sorel-tracy.qc.ca
http://sorel-tracy.qc.ca/~edouardb/
http://www.absolutearts.com/portfolios/e/edouardb/

----- Original Message -----
From:
To:
Sent: Thursday, July 19, 2001 11:05 AM
Subject: Re: Blue Lovers Only


> In my Quest for simple glazes i use ash a lot. mostly 50% ash 50% red
clay.
> Some i use red art some i use cave clay.
>
> I just did another test using 100 grms Plastic Vitrox and 100 Grms Ash. I
> added 3 grms of Cobalt Carb at cone 10 Reduction and wow is it a yummy
blue.
> I am using Highwaters Wonder White.
>
> If any body tries it let me know. I love blue
>
> Capt Mark
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

L. P. Skeen on thu 19 jul 01


OMG I need glasses....thought you were asking about Mark's personal
hygiene.....

L
----- Original Message -----
From: Edouard Bastarache
Subject: Re: Blue Lovers Only


> Hello Capt Mark,
> is your ash washed? If so, how many times?

Edouard Bastarache on fri 20 jul 01


LAFFFFFFFFF!!!



----- Original Message -----
From: L. P. Skeen
To:
Sent: Thursday, July 19, 2001 3:23 PM
Subject: Re: Blue Lovers Only


> OMG I need glasses....thought you were asking about Mark's personal
> hygiene.....
>
> L
> ----- Original Message -----
> From: Edouard Bastarache
> Subject: Re: Blue Lovers Only
>
>
> > Hello Capt Mark,
> > is your ash washed? If so, how many times?
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.