Jim Tabor on wed 11 jul 01


Inks CAN be made for hard surface glazes and are NOT limited to soft surfaces as was
stated in the post I sent on decals. I used a set of crystals bought from a lapidary
shop to do scratch tests for hardness when printing floor tiles.

The sentence in the fourth paragraph should read:

Glaze hardness and print hardness were sometimes a
factor. In other words, inks do NOT have to be limited to soft glazes.

If you need a drawing for the vacume table to print on, you can email me at:
taborj@earthlink.net