search  current discussion  categories  kilns & firing - manufacturers 

paragon kiln model b66

updated tue 10 jul 01

 

Kirk Morrison on sun 8 jul 01


I was giving a kiln I have been using for several years a Paragon B66, I need
to do a few minor repairs to the brick in it after the 60 mile move, what
else should I do after this move

Kirk

"Honor and Duty, First, Last and Always" R. E. Lee

Arnold Howard on mon 9 jul 01


If brick damage is cosmetic, I would not attempt to repair it. If
an element groove has come off, you can reattach the brick piece
with element staples.

Arnold Howard
Paragon

--- Kirk Morrison wrote:
> I was giving a kiln I have been using for several years a Paragon
> B66, I need
> to do a few minor repairs to the brick in it after the 60 mile
> move, what
> else should I do after this move
>
> Kirk
>
> "Honor and Duty, First, Last and Always" R. E. Lee
>
>
______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your
> subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.


__________________________________________________
Do You Yahoo!?
Get personalized email addresses from Yahoo! Mail
http://personal.mail.yahoo.com/