Could it be the rutile?
There are several beautiful blue glazes with more rutile than cobalt. When I
apply them on the bare piece I get green. When apply them above low alumina
glaze I get blue. I use it lately to get more coloring from the same
glaze.Like in this tile where I applied both ways!
http://members4.clubphoto.com/ababi306910/UTILITY__ClayArt/ The last
slide.

This is really nice.
Is this the "normal way" or it is because of "my" rutile?