search  current discussion  categories  glazes - misc 

glazing: geometric

updated thu 19 apr 01

 

Kurt Wild on wed 18 apr 01


All my work is done using "templates with various shapes cut into the
bendable plastic". Following the scratching of the design through the
unfired glaze, I stain the resultant areas with soluble salts. See my
article "Using soluble Colorants at Stoneware Temperatures" in the Sept.
1996, issue of Ceramics Monthly.

Also see my web site.

Kurt
Home/index: http://wwwpp.uwrf.edu/~kw77
Current work: http://wwwpp.uwrf.edu/~kw77/Available.html