On Thu, 12 Apr 2001 20:12:19 -0700, you wrote:

Anne,

That's going to be kind of touchy. Cone 016 will almost certainly burn
off the decoration. Cone 022 might make it. Firing in reduction will
help keep the hair from burning off (or can give interesting
ghosting), but I don't know if that's compatible with the conditions
for the lustres.

Good luck,

Bruce and Lynne Girrell