Joyce Lee on wed 11 apr 01


In fact, Mel, I went to a scholarship luncheon yesterday where each of
the place settings had a "miniature" molded vase in pastel colors ...
the micros would be at least 80% smaller and lighter than those vases.
These are REALLY little pots... afraid I might lose them in the firing,
actually. They're made of ^10 Tom Coleman's Bee Mix. May wind up with
pots that can only be viewed with a magnifier!