search  current discussion  categories  safety - toxicity 

toxic or not

updated mon 2 apr 01

 

wallace myers on sat 31 mar 01


Folks:

would some kind, knowledgeable person give me their opinion on whether =
it would be advisable to use the following glaze on food surfaces

30.0 flint
20.0 Custer feldspar
14.0 talc
31.5 gerst borate
5.0 EPK

Thanks
Wallace

Charles Moore on sun 1 apr 01


Wallace,

What cone are you firing to?

Charles
camoore33@earthlink.net
----- Original Message -----
From: "wallace myers"
To:
Sent: Saturday, March 31, 2001 2:26 PM
Subject: toxic or not


Folks:

would some kind, knowledgeable person give me their opinion on whether it
would be advisable to use the following glaze on food surfaces

30.0 flint
20.0 Custer feldspar
14.0 talc
31.5 gerst borate
5.0 EPK

Thanks
Wallace

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.