Dear Marianne,
Thanks for sending the results as it always exciting to hear what others =
are doing and getting for results with similar or same receipes, =
different corners of the planet.

The Wodo white is not a "hard white" like 5x20 with Zircopax. In my =
experience the dolomite gives the warmer tone. But that is only an =
eyeballing reference. I prefer a warmer white for most of my whites, but =
find Tony's 5x20 to be an excellent, look no further, liner glaze!

Many congrats to you for "jumping" and hopefully lots of successes in =
the future.
Best regards,
Alisa