another dumb one...cobalt carb

updated sat 24 mar 01

 

Andie Carpenter on wed 21 mar 01


Cobalt Question:

The last pound of cobalt carb I ordered was bright, bright pink. I
finally used it up, and the new pound I ordered is pink, but more like a
dusty rose color. I know they're different colors, as I compared the
bags.

Anyone know why this would be the case? Will it effect the glazes I use
it in?

Thanks!

: ) Andie

Steve Mills on fri 23 mar 01


Probably not, but ultimately remember the Potter's motto:

TEST IT FIRST!

:-)

Steve
Bath
UK


In message , Andie Carpenter writes
>Cobalt Question:
>
>The last pound of cobalt carb I ordered was bright, bright pink. I
>finally used it up, and the new pound I ordered is pink, but more like a
>dusty rose color. I know they're different colors, as I compared the
>bags.
>
>Anyone know why this would be the case? Will it effect the glazes I use
>it in?
>