Lynne Antone on wed 7 mar 01


<as a studio?? I would not put a kiln in, I don't think, because trailers
if they burn go jut like that (chimney effect.)>>

Lili and all,

I remember way back, probably longer back than I can reasonably guess,
someone had a large van that they took on the road to do clay outreach for
communities. They had quite a setup and the story I remember is that the van
was stolen, then in a later issue of a magazine, I think Ceramics Monthly, it
was recovered. Anyway, maybe someone else remembers this incident and knows
more how it all worked. This may even have been in the seventies.