search  current discussion  categories  glazes - cone 4-7 

cone 6r

updated thu 1 mar 01


Pancioli on wed 28 feb 01

Dear Clayarters:

Enough people responded about cone 6R glazes that I will post our best
results on the listserv after Spring Break. I can also bring the best of
the tests with me to NCECA if other Cone 6R people want to see them.

We began our testing with Marcia Selsor's fine list of glazes, posted on
the listserv a while back and again yesterday, and have grown it from
there. Thanks Marcia!!

I agree with Tom Sawyer that being able to see a photo of a glaze is
very helpful. Which brings me to the subject of Tom Sawyer.

He is an AMAZING guy of incredible energy, intellect, and heart. I was
privileged to meet him and stay at his home in Orlando. You will enjoy
meeting him at NCECA (he helps out at the Axner booth).