search  current discussion  categories  materials - misc 

gum printing on clay>>

updated wed 21 feb 01

 

Susan Maguire on tue 20 feb 01


Hi Susan Saunders........ I have just ordered Paul Scotts book. Will the
'gum printing' technique be explained in it or should I ask you to tell
all??

TIA


Susan Maguire On the Southeast Coast of Florida, USA
SCM333@Aol.Com

Susan Saunders on tue 20 feb 01


Hi Susan--the Scott book gives you a couple of pages about gum printing,
specific to ceramics. I have a bit more information from a workshop that I
took, with more specifics that have worked for me. I wrote another Clayarter
off list, suggesting that photo silkscreens might be a less complicated way
to go, but I'll be happy to send you my gum print xeroxes, by fax or
snailmail.

Susan Saunders