glaze request:^10 liner for raw-glazed soda-fired stoneware

updated thu 22 feb 01

 

Brian Molanphy on wed 21 feb 01


greetings,

i searched the archive (whew!) and didn't find references to recipes
for glazing leather-hard ware. i would like a liner for use on 'amador'
clay. a gloss white or cream, or a celadon. has anyone tried applying white
slip under red stoneware, then glazing celadon, in order to brighten the
color?
unglazed on the outside, 'amador' responds well to the soda. should
anyone care to suggest another commercially-available clay, i would be
interested in that too. -brian