search  current discussion  categories  glazes - misc 

new glaze has a name

updated fri 29 dec 00

 

will edwards on thu 28 dec 00


Hello,

Well I have had several to write me off-list to tell me to name that glaz=
e and
stick a label to it so I will.

Edward's 1234 Glossy ^6 (Like twelve thirty four)

Ferro Frit 3134 40.00
Epk Kaolin 30.00
Flint ( Quartz Silica ) 20.00 =

Wollastonite 10.00

I have some others that I will eventually get out there in time that will=
hold
those reds and yellows that are made with stains and sometimes raw materi=
als.
Purple is another one I have on hand if interested?
I also have made a data-bank for collecting results from those who test a=
ny of
the glazes I write with or without your use of calculations software. Tha=
t way
if you have some questions someone on here is bound to answer back and we=
can
hash it out over coffee. I will save the replies for reference and addtio=
nal
evaluation. Also they are archived thanks to our mayor who loves blue. "M=
el, I
am ready to be archived for awhile."
Calculation systems are a super tool. They are good only if the informati=
on in
them is correct and up-2-date with the materials you are currently using.=

The only positive way to end an argument is to lab test for extractable m=
etal
content such as boron/manganese/cobalt/copper/chromium or nickle.
Every ingredient listed above has FREE SiO2 in it. Don't breath the dust.=


William Edwards
The quickest way to an alchemist's heart is through his breast bone. But
chocolate is a close second!
=