About month or two I asked a question, because of losing too many pieces
while cleaning them.
Results: I fired to 630C 1166F, and cleaned the delicate pieces.The piece
that I cleaned with water, broke like it was unfired. the others I cleaned
mainly with steel wool but also other dry sharpeners, very good.
Thanks again for the direction!