: alumina hydrare on ifb

updated mon 11 dec 00

 

iandol on sun 10 dec 00


Dear Ted Banton=20

mixed with 1 gallon of aluminium paint that one could salt without =
damage to the IFB, any suggestions>

Get an old IFB and put a coat on the top and half way down the sides, =
Find a kind person with as salt kiln which is used regularly and ask =
them if they would cooperate by firing it about ten times positioned =
where it would get a lot of heat and salt.

Note the results and let us all know.