Go to Feldspar Corperation on the net and they list the full spectrum of=

their spars. Its the best way to keep up to date with the analysis.
Here is what I have for Unity Molecular Formula that I had in my old
records..

0.265 K2O 0.998 Al2O3 5.776 SiO2
0.578 Na2O 0.001 Fe2O3 0.157 CaO

William Edwards