terra sig - old recipe wanted

updated wed 6 dec 00

 

Bill and Sylvia Shirley on tue 5 dec 00


It's been discussed many times recently, but I'm unable to
find a recipe in the archives. Can somebody please give the
recipe for terra sig, using the calgon chemical (sodium
hexametaphosphate). I bought some from Dharma Trading Co.

Thanks,

Sylvia Shirley

lela martens on tue 5 dec 00


To Sylvia, I don`t know if these are the ones you mean. They were sent to
me from June Macdonald.
Terra Sig Gold Art 500g.
Water 1 kilo
Calgon 3g

or
Red Art 2 kilo
Water 8 kilo
Calgon 1-3 g. Lela


>From: Bill and Sylvia Shirley
>Reply-To: Ceramic Arts Discussion List
>To: CLAYART@LSV.CERAMICS.ORG
>Subject: terra sig - old recipe wanted
>Date: Tue, 5 Dec 2000 12:35:34 -0600
>
>It's been discussed many times recently, but I'm unable to
>find a recipe in the archives. Can somebody please give the
>recipe for terra sig, using the calgon chemical (sodium
>hexametaphosphate). I bought some from Dharma Trading Co.
>
>Thanks,
>
>Sylvia Shirley
>
>_____________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.

_____________________________________________________________________________________
Get more from the Web. FREE MSN Explorer download : http://explorer.msn.com

Bill and Sylvia Shirley on tue 5 dec 00


Lela,

Thanks a million. That's just what I was looking for.

Sylvia