Puddy & Co. on tue 5 dec 00


Charles,
sorry, I should be more specific. It is a soda feldspar available from
our Pottery Supply House in Ontario. I do not know its' chemical
composition or the place of origin, but this should be available from
the supplier. I do not remember whether the original recipe was calling
for this particular felspar, or any other soda feldspar. I suppose it
may matter seing that there is 43% if it in the recipe. This one worked
nicely though. I wish you happy testing

Hanna Lewandowski