clennell on thu 23 nov 00


I don't know about purple shino but i do know that a fellow potter Larry
Davidson used to make a glaze called bubblegum. It was a shino with a high
alumina pink stain added. Knowing Larry he just added it by eyeballing it.
Probably a high temperature purple stain could be added the same way to
shino. Junkyard Dawg uses alot of stains and will probably give a right on
answer to your enquiry.
Double Bubble and Thrills shino. This could be a yuppie trend in the making.
Best of luck,
tony

sour cherry pottery
tony and sheila clennell
4545 king street
beamsville, on.L0R 1B1
http://www.sourcherrypottery.com
clennell@vaxxine.com