In response to the question about who is making sushi plates:

I hand form them from slabs using a plaster hump mold made from the
interior of a large wok. I also extrude them and ram press them. The
extruded and pressed ones have the feet incorporated into the die or mold.
You can see some at my web site: www.hominid.net/chris.htm
regards to all,
Chris Henley