paperclay, not as dry as it looks.

updated tue 10 oct 00

 

Marcia Selsor on mon 9 oct 00


Dear Alisa,
I always fire paperclay slowly to let all the fumes/smoke out of the
kiln.
I do sculpture and raku slabs in paperclay and I love it. But fire
slower than regular clay. I leave the lid open until I turn on the "high switch.
Marcia in Montana