Kurt Wild on sat 14 oct 00


4 hours 20 minutes (reduction fire) after candling all night.
Top and bottom cones even 9 flat. Haven't fired that even in a long
time. Must have stacked it well.
Used 2 gallons propane per cubic foot, 10 cu. ft. setting space.
I know that the ITC 100 and 296 top coat helped on fuel use.
As Bernard Leach said in the old film most of us have seen: "Kiln's alright!"

Can't wait to see the pots - it's been forever since last March when I
fired last!
Kurt