Wade Blocker on fri 29 sep 00


Luis,
If you put no glaze on yur bonsai posts there is no reason why you could
not fire the pots in one firing. The only thing you might have to consider
is to fire slowly in the beginning as you would in any bisque firing, and
then fire as you would in a gloss or glaze firing. Mia in ABQ