Hello Carolyn -
The finest gauge wire that we have on hand is 27g Nichrome wire. =
The next gauge up is 23g then 20g. The 27g is very fine, you could do =
very detailed metal work with this. It is a bit too fine to make an =
earring hoop from. The wire sells for $2.30 US per metre (3 feet). You =
can also buy by the pound. =20

Regards,
Shannon O'Brien
Euclid Kilns & Euclid's Elements
1-800-296-5456
www.euclids.com